Eliminates mesh degreasing:
- Just rinse with water
- No cleaning agents necessary
- Cost and time savings
- Less environmental burden
SEFAR PET 1500: uniform wetting
|
|
|
 |
Wetting Test:
Rinsing with blue dyed water shows clearly
the difference in the wetting behavior
Mesh without surface treatment: uneven
wetting |
|
|
 |
Improved adhesion
of stencil material
- Optimal retaining of screen dots and
fine lines
- Considerable prolongation of stencil
life
SEFAR PET 1500: no remaining of emulsion
on adhesive tape
|
|
|
 |
Tape
Test: An adhesive tape is fixed
across the stencil
Mesh without surface treatment: parts of
the emulsion are remaining on the tape
|
|
|
 |
Improved printing results
- Even and constant ink deposit
- High-quality printing results
SEFAR PET 1500: homogeneous ink deposit
|
 |
Printing on a black
background
This highly magnified picture shows clearly
the difference of the ink deposit
Mesh without surface treatment: uneven ink
deposit, the background is partly visible
|
|